Several important Australian Federal Government buildings located in the Parliamentary Triangle in Canberra were constructed using galvanized reinforced pre-cast cladding, window and facia units.  A 26 year life assessment of the buildings stated that “throughout the building facade there is no rusting, cracking or spalling of concrete“.